Weathering Steel Plate

Send Inquiry
Weathering Steel Plate
Details
Weathering steel plate is a high-strength, low-alloy structural steel designed to form a protective oxide layer (patina) under atmospheric exposure.
Category
Steel Plate & Sheet
Share to
Description

Weathering steel plate is a high-strength, low-alloy structural steel designed to form a protective oxide layer (patina) under atmospheric exposure. Through alternating wet/dry cycles over 18–36 months, the surface develops a dense, amorphous inner layer ($\alpha$-FeOOH) enriched with Cu, Cr, Ni, and P. This passivated barrier reduces terminal corrosion to < 10 µm/year, eliminating the need for paint or galvanizing in ISO 9223 C1–C3 environments and extending service life beyond 100 years.

 

Key Product Characteristics

 

Self-Passivating Layer: Forms a tight $\alpha$-FeOOH barrier in 18–36 months, stopping sub-surface corrosion.


Superior Corrosion Resistance: 4x–8x higher atmospheric corrosion resistance than standard carbon steels (e.g., A36, S235JR).


High Strength: Minimum yield strength of 345 MPa (50 ksi) for thicknesses up to 100 mm, enabling structural weight reduction.


Durable Performance: Retains fatigue endurance and impact toughness (≥ 27 J at -20°C standard) after patina stabilization.

 

Technical Specifications

 

Chemical Composition (Heat Analysis, wt%)

 

Grade

C

Si

Mn

P

S

Cr

Cu

Ni

V / N / Nb

ASTM A588 Gr. A

≤ 0.19

0.30–0.65

0.80–1.25

≤ 0.040

≤ 0.050

0.40–0.65

0.25–0.40

≤ 0.40

V: 0.02–0.10

ASTM A242 Type 1

≤ 0.15

0.15–0.75

≤ 1.00

0.07–0.15

≤ 0.050

0.30–1.25

0.25–0.55

≤ 0.65

-

S355J2WP (EN 10025-5)

≤ 0.12

≤ 0.75

≤ 1.00

0.06–0.15

≤ 0.035

0.30–1.25

0.25–0.55

≤ 0.65

N: ≤ 0.009

S355J2W (EN 10025-5)

≤ 0.16

≤ 0.50

0.50–1.50

≤ 0.035

≤ 0.035

0.40–0.80

0.25–0.55

≤ 0.65

Zr/Nb options

Corten A

≤ 0.12

0.25–0.75

0.20–0.50

0.07–0.15

≤ 0.030

0.50–1.25

0.25–0.55

≤ 0.65

-

Corten B

≤ 0.19

0.30–0.65

0.80–1.25

≤ 0.040

≤ 0.030

0.40–0.65

0.25–0.40

≤ 0.40

V: 0.02–0.10

 

Mechanical Properties

 

Standard & Grade

Nominal Thickness (t)

Min. Yield Strength (ReH)

Tensile Strength (Rm)

Min. Elongation (A5)

Charpy V-Notch Impact Test

ASTM A588

t ≤ 100 mm (4 in)

345 MPa / 50 ksi

485 MPa / 70 ksi

21% (in 200 mm)

Optional (27 J @ -20°C)

ASTM A242

t ≤ 19 mm (0.75 in)

345 MPa / 50 ksi

485 MPa / 70 ksi

21% (in 200 mm)

N/A

S355J2WP

t ≤ 12 mm

355 MPa

470–630 MPa

20%

27 J @ -20°C

S355J2W

t ≤ 16 mm

16 < t ≤ 63 mm

63 < t ≤ 100 mm

355 MPa

345 MPa

335 MPa

470–630 MPa

470–630 MPa

470–630 MPa

22%

22%

21%

27 J @ -20°C

S355K2W

t ≤ 100 mm

335–355 MPa

470–630 MPa

20%

40 J @ -20°C

 

Dimensional Tolerances & Supply Range

 

Parameter

Standard Range

Custom / Option

Thickness

2.0 mm – 100 mm

Up to 150 mm

Width

1,000 mm – 3,200 mm

Up to 4,000 mm

Length

2,000 mm – 12,000 mm

Up to 18,000 mm

Flatness Tolerance

EN 10029 Class N / ASTM A6

Class S (Restricted)

Thickness Tolerance

EN 10029 Class B / ASTM A6

Half-standard tolerance available

 

Grades & Standards Summary

 

ASTM A588 / Corten B: Low-phosphorus grades for heavy load-bearing structural members, bridges, and welded structures.


ASTM A242 / Corten A: High-phosphorus grades suitable for thin architectural panels (t ≤ 19 mm) requiring rapid weathering. Not for heavy structural welds.


EN 10025-5 Series:

  • S355J2WP: High-P architectural grade (t ≤ 12 mm).
  • S355J2W: Low-P structural grade for welded bridges and buildings (t ≤ 100 mm).
  • S355K2W: High-impact strength grade designed for cold climates (40 J at -20°C).

 

Surface & Processing Options

Surface States

As-Rolled: Standard mill finish. Mill scale should be removed to ensure uniform weathering.
Shot-Blasted (Sa 2.5): Cleaned surface for accelerated and even patina development.
Pre-Patinated: Chemically treated post-blasting to produce a uniform rust finish in 3–7 days.

 

Fabrication & Welding

Cutting: Suitable for Laser, Plasma, and Oxy-fuel cutting (preheat to 100–150°C for thickness > 40 mm).
Cold Bending: Recommended inner radius R/t ≥ 2.5 (transverse) and R/t ≥ 3.5 (longitudinal).
Welding: Standard SMAW, GMAW, FCAW, and SAW methods.
Single-Pass: Standard fillers (e.g., E7018) can be used due to dilution.
Multi-Pass: Use matching weathering fillers (e.g., AWS E8018-W1) to ensure joint corrosion resistance.

 

Applications & Environmental Limits

Applications

  • Bridges, highway structures, and architectural facades.
  • Shipping containers, rail cars, hopper wagons, and industrial exhaust ducts.
 

Environmental Limitations

  • Unsuitable for marine splash zones or continuous saltwater immersion.
  • Not recommended for constantly damp microclimates or heavy de-icing chemical spray zones.
 

Quality Control & Certification

 

Quality Workflow: Heat Testing ➔ Ultrasonic Inspection (EN 10160 / ASTM A578) ➔ Mechanical/Impact Testing ➔ Mill Test Certificate (EN 10204 3.1).


Testing Methods: Optical Emission Spectrometry (Chemical Analysis), ISO 6892-1 / ASTM A370 (Tensile), ISO 148-1 / ASTM E23 (Impact down to -40°C).


Traceability: All plates are heat-traceable and supplied with EN 10204 3.1 or 3.2 MTCs (third-party inspection by SGS, TÜV, or BV available).

 

Customization, Packaging & Delivery

Processing

CNC plasma/laser cutting, edge beveling (V/X/K/J preps), drilling, and bending.

Packaging

Heavy-duty steel strapping, VCI anti-rust paper wrap, wooden skid supports, and edge protectors.

Logistics

Containerized (20ft GP / 40ft GP / OT) or Breakbulk shipments (FOB, CFR, CIF, DDP).

 

Quote Request Guide

Request a Technical Quote / RFQ
Grade & Standard: [ E.g., ASTM A588 Grade A / S355J2W ]
Dimensions (Thickness x Width x Length): [ E.g., 10 mm x 2000 mm x 6000 mm ]
Total Quantity: [ Metric Tons / Pieces ]

Surface Condition: [ As-Rolled / Shot-blasted Sa 2.5 / Pre-Patinated ]
Processing / Fabrication Needs: [ Cutting / Beveling / Drilling / None ]
Destination Port & Incoterms: [ E.g., CIF Hamburg / FOB Tianjin ]
Attach Drawings / Specifications (Optional): [ Choose File ]

 

FAQ

 

Q: What is the main difference between Corten A and Corten B / A588?

A: Corten A / A242 has higher phosphorus for faster weathering in thin architectural panels (t ≤ 19 mm). Corten B / A588 / S355J2W has lower phosphorus, offering better weldability and impact toughness for heavy structural loads (t ≤ 100 mm).

Q: How long does natural patina formation take?

A: It takes 18 to 36 months under natural outdoor wet/dry cycles. Chemical treatment can shorten initial color formation to 3–7 days.

Q: Is weathering steel suitable for coastal environments?

A: No. High chloride concentration prevents the formation of the protective oxide layer, causing continuous corrosion.

Q: Does weathering steel require special welding filler wire?

A: Yes, multi-pass welds require weathering-rated filler metals (e.g., AWS E8018-W1) to maintain corrosion resistance across the joint.

Q: Why should mill scale be removed before installation?

A: Mill scale detaches unevenly over time, resulting in a patchy and non-uniform rust appearance. Shot blasting to Sa 2.5 ensures even weathering.

Hot Tags: weathering steel plate, China weathering steel plate manufacturers, suppliers, factory

Send Inquiry